JN Alloy huwa l-ikbar stockiest tal-fornitur tal-pjanċa Incoloy 800h b'inventarju enormi ta 'liga 800h pjanċa rrumblata sħuna, ASTM B409 Plate Plused UNS N08810 u Pjanċa Rolled Cold Incoloy 800H. Noffru DIN 1.1958 / 1.4876 kolji b'diversi daqsijiet bl-aħjar prezz. Aħna l-manifattur ewlieni ta 'Incoloy Alloy 800h Strip & Incoloy 800h folja.
Incoloy 800H is an iron-nickel-chromium alloy having the same basic composition as Incoloy 800, with significantly higher creep rupture strength. Sheets and plates made of Incoloy 800H have a stiff structure, contributing to increased temperature stability. They contain aluminum and titanium, providing corrosion resistance and preventing carburization precipitation in heat-working applications. Sheets and plates made of Incoloy 800H offer excellent erosion, corrosion, and oxidation resistance in media and perform well in applications involving constant high temperatures. The higher strength results from close control of carbon, aluminum and titanium contents in conjunction with a high temp anneal. The 800H modification was to control carbon (0.05 to 0.10%) and grain size to (>ASTM 5) biex jottimizzaw il-proprjetajiet ta 'ksur tal-istress. INCOLOY 8 0 0H għandu aktar modifiki għal-livelli ta 'titanju u aluminju kkombinati (0.85 sa 1.2%) biex jiżguraw proprjetajiet ottimali ta' temperatura għolja. Il-liga hija ċċertifikata doppja u tgħaqqad il-proprjetajiet taż-żewġ forom. Pjanċa ta '800h Incoloy ma ssirx imsaħħaħ anke wara użu fit-tul tal-liga bejn il-firxa tat-temperatura ta' 1200 - 1600 grad F, f'liema stadju ħafna gradi tal-azzar li ma jissaddadx għandhom it-tendenza li jsiru fraġli.
Il-ligi JN jipprovdu l-aħjar pjanċa ta '800h Incoloy. Aħna fornituri tal-aqwa folji u pjanċi tal-azzar Incoloy 800h. Dawn il-folji u l-pjanċi huma manifatturati mill-liga tal-istainless steel Incoloy 800h, li għandha ħafna mill-akbar proprjetajiet. Dan jagħmilhom l-iktar utli għal applikazzjonijiet robusti industrijali. Dawn il-folji u pjanċi għandhom saħħa ogħla u reżistenza superb. Dawn il-pjanċi jikkonsistu minn nikil u kromju. Bil-preżenza ta 'dawn l-elementi, dawn il-pjanċi tal-liga ta' 800h isiru aktar reżistivi għall-korrużjoni minħabba fatturi differenti bħall-korrużjoni, l-umdità, u l-kimiċi. Dawn il-folji tal-pjanċi Incoloy 800h huma ta 'natura duttili u malleabbli ħafna. Għandhom ukoll saħħa tat-tensjoni akbar u saħħa tar-rendiment. Għalhekk, ma għandhom l-ebda qsim. Huma wkoll reżistivi għall-bidla tal-proprjetajiet f'temperatura ogħla. Aħna qed nipprovdu wkoll il-kwalità superjuri tal-folji u l-pjanċi lill-klijenti kollha disponibbli madwar id-dinja. Fost l-istokk, aħna fost l-istokk ta 'min jafdaha u l-esportatur tal-kwalità tal-folji u l-pjanċi.
Speċifikazzjoni tal-pjanċa Incoloy 800h
|
Speċifikazzjonijiet |
ASTM B409 / ASME SB409 |
|
Speċifikazzjoni Dimensjonali |
JIS, AISI, ASTM, GB, DIN, EN, eċċ |
|
Wisa ' |
1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, eċċ |
|
Ħxuna |
4mm -100 mm |
|
Tul |
2000mm, 2440mm, 3000mm, 5800mm, 6000mm, eċċ |
|
Finitura tal-wiċċ |
2b, 2d, ba, no.1, no.4, no.8, 8k, mera, checkered, imqabbża, linja tax-xagħar, blast tar-ramel, pinzell, inċiżjoni, pjanċa rrumblata sħuna (HR), folja rrumblata kiesħa (CR), satin (iltaqa 'ma' plastik miksija) eċċ. |
|
Ebusija |
Artab, iebes, nofs iebes, kwart iebes, rebbiegħa iebsa eċċ. |
|
Forma |
Kojls, fuljetti, rombli, folja sempliċi, folja shim, folja mtaqqba, pjanċa mżewqa, strixxa, flats, vojta (ċirku), ċirku (flanġ) eċċ. |
|
Finitura tal-wiċċ |
Nru.1, Nru.4, Nru.8 Mera Temm, 2B |
Incoloy 800h Plate, Sheet & Coil Chemical Composition
|
Grad |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
Al |
Ti |
|
800H |
0.05 – 0.10 |
1.50 Max |
1. 00 Max |
0. 015 Max |
0. 75 Max |
39.50 min |
30.00 – 35.00 |
19.00 – 23.00 |
0.15 – 0.60 |
0.15 – 0.60 |
ASTM B409 UNS N08810 Propjetajiet Mekkaniċi tal-Pjanċa
|
Element |
Densità |
Punt ta 'tidwib |
Qawwa tat-tensjoni |
Qawwa tar-rendiment (0. 2% offset) |
Titwil |
|
800H |
7.94 g / cm3 |
1385 grad (2525 grad F) |
Psi - 75, 000, MPA - 520 |
Psi - 30, 000, MPA - 205 |
30 % |
Materjal ekwivalenti ta 'inconel 800h Plate
|
Standard |
Werkstoff nr. |
Uns |
JIS |
BS |
Gost |
Afnor |
En |
Jew |
|
Incoloy 800h |
1.4958 / 1.4876 |
N08810 |
NCF 800h |
Na 15 (H) |
ЭИ670 |
Z8nc 33-21 |
X5nicralti 31-20 |
XH32T |
Applikazzjonijiet Incoloy Alloy 800h
Bojlers tal-Qtugħ tal-Furnazz tal-Etilene
Proċessar kimiku u petrokimiku
Qsim tal-idrokarburi
Super-heater u jerġgħu jsaħħu fl-impjanti tal-enerġija
Valvi, fittings u komponenti oħra esposti għal attakk korrużiv minn 1100-1800 grad f
Bastimenti tal-pressjoni
Fran industrijali
Skambjaturi tas-sħana
Tagħmir li jittratta s-sħana