JN ALLOY supplies Hastelloy c2000 Pipe, ASTM B622 UNS N06200 Tube, Hastelloy Alloy c2000 Tube, 2.4675 Hastelloy c2000 Tube, Hastelloy c2000 Tube, Alloy c2000 Pipe, Hastelloy c2000 Pipe, Alloy c2000 Material, Hastelloy c2000 Price, N10665 Tube, Alloy c2000 Tube, Hastelloy c2000 Tubing, Alloy c2000 Seamless Tubing .
Hastelloy C2000 pipe is corrosion resistant alloy with excellent corrosion resistance to oxidizing environments. Hastelloy C2000 Tube has great resistance to stress corrosion cracking. Alloy C2000 Tube made by nickel-chromium-molybdenum(Ni-Cr-Mo). Hastelloy C2000 Tube mostly use in the Chemical Process Industries. Hastelloy C-2000 Welded Tube is an extremely versatile nickel alloy resistant to corrosion in all acids and chloride solutions, over wide temperature ranges. Hastelloy C2000 Seamless Pipes broadens the range of the nickel-chromium-molybdenum alloy family with the addition of copper which allows for resistance to an extensive range of corrosive chemicals including sulfuric, hydrochloric, and hydrofluoric acids over large temperature ranges. Nickel Alloy C2000 Tube has poor corrosion resistance to oxidizing environments, therefore, it is not recommended for use in oxidizing media or in the presence of ferric or cupric salts because they may cause rapid premature corrosion failure. Alloy C2000 Seamless Tubing is a copper-bearing Ni-Cr-Mo material with exceptional resistance to sulfuric acid.Alloy C2000 Seamless Pipes has outstanding resistance to Sulfuric Acid, Hydrofluoric Acid, Hydrochloric Acid, Phosphoric Acid, Chlorides, Organic Acids, Alkalis, Crevice Corrosion, Pitting, Stress Corrosion Cracking, etc.
Jinie Technology (Jiangsu) Co., LTD exports a wide range of Hastelloy C2000 Tube, which performs brilliantly in large temperature and concentration ranges. Hastelloy Alloy C2000 Seamless Tubing is stiffer than most austenitic stainless steels, and more energy is required during cold forming. ASTM B626 Alloy C2000 Seamless Tubing also has a high chromium content, to maximize its resistance to oxidizing chemicals and process streams contaminated with ferric ions and dissolved oxygen. The specified Carbon content across Hastelloy C2000 EFW Tubes is 0.015 percent at the max, and Silicon content of 0.10 percent max. The quenching by water after the complete solution annealing of Hastelloy C2000 ERW Pipes is preferred for cold processed alloy prior to welding. These are very good oxidation and carburization resistance. Hastelloy C2000 Welded Tubes is resistant to an extensive range of corrosive chemicals including sulfuric, hydrochloric & hydrofluoric acids. The weld metal like this is viscous and some torch manipulation is usually necessary. Whether you need on-demand delivery of finished, end-use technical support or a partner with global presence, we provide value far beyond the alloys themselves.
Hastelloy C2000 Pipes & Tubes Specification
|
|
ASTM B619, ASTM B622 / ASME SB619, ASME SB622, ASTM B 619; ASME SB 619 (Welded); ASTM B 622; ASME SB 622 (Seamless); ASTM B626; ASME SB626 (Welded Tube). |
|
Hastelloy C2000 Seamless Tube Size |
3.35 mm OD To 101.6 mm OD |
|
Hastelloy C2000 Welded Tube Size |
6.35 mm OD To 152 mm OD |
|
|
10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg. |
|
Hastelloy C2000 tubing wall thickness |
{{0}}.020" –0.220", (special wall thicknesses available) |
|
Alloy C2000 tube Length |
|
|
Hastelloy Alloy C2000 Tube Finish |
|
|
Hastelloy C2000 tube Form |
|
|
Hastelloy C2000 Tube Type |
|
|
|
|
|
|
All Hastelloy Alloy C2000 tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer's request.) |
|
|
|
|
|
|
|
|
Hastelloy C2000 Capillary Tube & Other Odd Size |
|
|
|
|
Manufacturers of Hastelloy C2000 Tubes & Tubing |
ASTM B622 Hastelloy C-2000 Seamless Pipe & Tube Chemical Composition
|
|
|
|
|
|
W |
|
|
C |
V |
P |
|
|
Hastelloy C2000 |
15.0-17.0 |
14.5-16.5 |
4.0-7.0 |
3.0-4.5 |
2.5 max |
1.0 max |
.01 max |
.35 max |
.04 max |
.08 max |
ASME SB626 Hastelloy C2000 Welded Tubing Mechanical Properties
|
|
|
|
|
|
Hastelloy C2000 |
690 MPa |
310 MPa |
45% |
Hastelloy C2000 Seamless Pipes Equivalent Grades
|
|
|
|
|
|
Hastelloy C2000 |
2.4675 |
N06200 |
NW 6200 |